Exaton

Exaton NiCrMo-10

The following items have been added to your list


x

NiCrMo-10 is a NiCrMo alloy of type alloy UNS N06022. It is a versatile alloy with excellent wet corrosion resistance in oxidizing and reducing media. It has better overall corrosion resistance than other NiCrMo alloys such as alloy UNS N10276 (2.4819) and alloy UNS N06626 (2.4856). However, in severely reducing media alloy UNS N10276 is preferred where NiCrMo-10 is a better matching consumable. NiCrMo-10 is used for joining alloy UNS N06022 (2.4602) and is widely used as overmatching filler material for alloy UNS N10276 (2.4819) and other nickel-chrome-molybdenum alloys for better weld metal properties. Typical applications for NiCrMo-10 are found in components for organic synthesis, flue gas scrubber systems, electrolytic galvanizing, plate heat exchangers, phosphoric acid production, wet chlorine gas, hypochlorite and chlorine dioxide atmosphere. NiCrMo-10 is also used in combustion-resistant components for high pressure oxygen service and ferric and cupric chloride environments.

BUY NOW


Typical Charpy V-Notch Properties

As Welded
Impact Value 33 ft-lb
Impact Value 45 J
Shielding Gas ISO
Testing Temperature -321 °F
Testing Temperature -196 °C

Typical Tensile Properties

ConditionElongationShielding GasTensile Strength Yield Strength
As Welded36 %ISO760 MPa (110 ksi)510 MPa (74 ksi)

Deposition Data

Deposition Rate @ 90% I max Diameter Deposition Efficiency (%) Number of electrodes/kg weld metal
41 sec 0.9 kg/h (2,0 lb/h) 2.5 x 300.0 mm (0.098 x 11,8 in.) 66 % 103
44 sec 1.2 kg/h (2,6 lb/h) 3.2 x 300.0 mm (1/8 x 11,8 in.) 69 % 56
71 sec 2.2 kg/h (4,9 lb/h) 4.0 x 350.0 mm (5/32 x 13,8 in.) 67 % 30

Classifications

Classifications SFA/AWS A5.11 : ENiCrMo-10
EN ISO 14172 : E Ni 6022

Consumable Characteristics

Alloy Type Ni-based CrMo
Coating Type Basic
Welding Current DC+

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Co Cr Cu Fe Mn Mo Ni P S Si V W
0.02 % 0.25 % 21 % 0.04 % 4 % 0.5 % 14.0 % 57 % 0.010 % 0.007 % 0.15 % 0.07 % 3 %