CORE-BRIGHT 316L

CORE-BRIGHT 316L

Welds types 316, 316L and 318 steels. Contain 2-2.5% molybdenum to increase the corrosion resistance to pitting induced by sulfuric and sulfurous acids, sulphites, chloride, and cellulose solutions. Used extensively in the rayon, dye, and paper industries.

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 42 % 87 ksi 62 ksi

Typical Weld Metal Analysis %

MnMoCSiFerriteNiCr
1.30 %2.20 %0.03 %0.70 %7 FN %12.50 %19.70 %

Approvals: ASME SFA 5.22; AWS A5.22; E316LTO-3; CERTIFIED BY C.W.B.- AWS A5.22
Classifications: AWS A5.22; E316LT0-3

Approvals are based on factory location. Please contact ESAB for more information.


x
CORE-BRIGHT 316L

Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 42 % 87 ksi 62 ksi

Typical Weld Metal Analysis %

MnMoCSiFerriteNiCr
1.30 %2.20 %0.03 %0.70 %7 FN %12.50 %19.70 %

Approvals: ASME SFA 5.22; AWS A5.22; E316LTO-3; CERTIFIED BY C.W.B.- AWS A5.22
Classifications: AWS A5.22; E316LT0-3

Approvals are based on factory location. Please contact ESAB for more information.


x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : CORE-BRIGHT 316L
CB 316L 3/32X55#CL 35ST24120V Buy Local
CB 316L 2.0X22.7KG CL 521913327 Buy Local
CB 316L 3/32X50#CL 251933305 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..