A positional rutile wire for the welding Ni-Cr-Mo alloys with 80% Ar + 20% CO2 shielding gas.

BUY NOW


Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
Element Nb C Si Mn Cr Mo Ti Fe Nb+Ta
Nominal Percentage 3.8 % 0.023 % 0.36 % 0.24 % 21.89 % 8.63 % 0.18 % 0.52 % 3.57 %

Typical Charpy V-Notch Properties

Conditional Statement As welded
Impact Value (imp) 55 ft-lb
Impact Value (met) 75 J
Testing Temperature 0 degC (32 degF)
Conditional Statement As welded
Impact Value (imp) 52 ft-lb
Impact Value (met) 70 J
Testing Temperature -196 degC (-321 degF)

Classifications

Grade ENiCrMo3T1-4
Name AWS A5.34
Grade T Ni 6625 P M 2
Name EN ISO 12153

Consumable Characteristics

Welding Current DC+
Alloy Type Ni-Cr-Mo

Typical Tensile Properties

ElongationTensile Strength (imp)Yield Strength (imp)
42 %788 MPa (114 ksi)501 MPa (73 ksi)

Deposition Data

Wire Feed Speed 5.8-13.8 m/min
Wire Feed Speed 228-543 in./min
Voltage 23-32 V
Diameter 1.2 mm
Diameter .045 in.
Deposition Rate 1.9-4.2 kg/h
Deposition Rate 4.2-9.3 lb/h
Current 130-210 A
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Shield-Bright NiCrMo-3
SB NICRMO-3 045X33# VP 35ZA12982V FIND A DISTRIBUTOR
SB NICRMO-3 045X11# VP 35ZA1298XX FIND A DISTRIBUTOR
x
x

x

Loading..