Coreshield 8-Ni1 H5 is a self-shielded flux cored wire designed to produce welds with low diffusible hydrogen and robust mechanical properties. It is welder friendly and has excellent all-position welding operability. Using DCEN polarity, it produces nice weld beads by either up-hill or down-hill welding to suit for a wider range of WPS requirements. Coreshield 8-Ni1 H5 is especially suited for making root passes or handling poor fit-up, and it features a diffusible hydrogen content lower than 5.0 ml/100g. Coreshield 8-Ni1 H5 can be ideally used in critical steel applications, such as offshore TKY joints, pipe structures, bridges, storage tanks and other applications where cold-cracking resistance is preferred.

BUY NOW


Industries

  • Offshore Oil
  • Bridge Construction
  • Mobile Equipment
  • Civil Construction
  • Industrial and General Fabrication
  • Ship/Barge Building

Welding Process

  • FCAW (Flux Core)

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 30 % 78 ksi 65 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 110 ft-lb -20 °F
As Welded 108 ft-lb -40 °C

Typical Weld Metal Analysis

weld metal analysis
PMnMoCuSCNbVSiNiAlCr
0.008 %1.4 %0.01 %0.04 %0.008 %0.02 %0.003 %0.008 %0.35 %1.00 %0.75 %0.04 %

Classifications: ASME SFA 5.36; ASME SFA 5.29; AWS A5.36; E71T8-A4-Ni1; AWS A5.29; E71T8-Ni1-J

Alloy Type: Low Alloy 1%Ni
Diffusible Hydrogen: <5 ml/100g
Welding Current: DC-
x

Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 30 % 78 ksi 65 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 110 ft-lb -20 °F
As Welded 108 ft-lb -40 °C

Typical Weld Metal Analysis

weld metal analysis
PMnMoCuSCNbVSiNiAlCr
0.008 %1.4 %0.01 %0.04 %0.008 %0.02 %0.003 %0.008 %0.35 %1.00 %0.75 %0.04 %

Classifications: ASME SFA 5.36; ASME SFA 5.29; AWS A5.36; E71T8-A4-Ni1; AWS A5.29; E71T8-Ni1-J

Alloy Type: Low Alloy 1%Ni
Diffusible Hydrogen: <5 ml/100g