ESAB

Coreshield 8

The following items have been added to your list


x

An all positional self-shielded cored wire ideal for welding outdoor structural steelwork.

BUY NOW


Typical Charpy V-Notch Properties

as welded

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded24 %565 MPa (82 ksi)465 MPa (67 ksi)

Deposition Data

Current Deposition Rate Diameter Deposition Efficiency (%) Wire Feed Speed
200 A 2.8 kg/h (6.13 lb/h) 1.8 mm (0.072 in.) 79.4 % 406 cm/min (160 in./min)
225 A 3.3 kg/h (7.32 lb/h) 1.8 mm (0.072 in.) 80.3 % 483 cm/min (190 in./min)
155 A 1.9 kg/h (4.16 lb/h) 1.6 mm (1/16 in.) 78.6 % 381 cm/min (150 in./min)
180 A 2.3 kg/h (5.14 lb/h) 1.6 mm (1/16 in.) 79.6 % 470 cm/min (185 in./min)
205 A 3.0 kg/h (6.60 lb/h) 1.6 mm (1/16 in.) 78.2 % 610 cm/min (240 in./min)
220 A 3.4 kg/h (7.53 lb/h) 1.6 mm (1/16 in.) 78.9 % 698 cm/min (275 in./min)
150 A 1.8 kg/h (3.96 lb/h) 2.0 mm (5/64 in.) 80.6 % 229 cm/min (90 in./min)
175 A 2.2 kg/h (4.83 lb/h) 2.0 mm (5/64 in.) 80.9 % 279 cm/min (110 in./min)
200 A 2.7 kg/h (5.93 lb/h) 2.0 mm (5/64 in.) 80.4 % 343 cm/min (135 in./min)

Classifications

Classifications ASME SFA 5.36 :
ASME SFA 5.20 :
AWS A5.36 : E71T8-A2-CS3-H8
AWS A5.20 : E71T-8 JD-H8

Approvals

Approvals ABS
BV
CWB CSA W48 E491T-8-H8
DB
DNV-GL
LR
Seismic Certified "D"
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type C Mn
Shielding Gas None
Welding Current DC-

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
Al C Mn P S Si
0.51 % 0.19 % 0.44 % 0.010 % 0.003 % 0.15 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Coreshield 8
249946609 Find a distributor
14C816463V Find a distributor
242206704 Find a distributor
242206746 Find a distributor
242206357 Find a distributor
242206450 Find a distributor
242206449 Find a distributor

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..