Coreshield 11

The following items have been added to your list


x

Coreshield 11 is an all-position self-shielded flux cored welding wire meeting all requirements for the E71T-11 classification. Coreshield 11 is excellent for use on single or multiple pass lap, fillet and butt welds on mild steels in all welding positions. Limitations do exist for multipass welds in excess of 1/2 in (12.7 mm). It produces smooth arc action, full slag coverage, easy slag removal, and low spatter. This product should find excellent acceptance in general purpose mild steel fabrication. In structural fabrication, the product can be used where no seismic requirements are present. Coreshield 11 is run DCEN.

BUY NOW


Industries

  • Automotive
  • Civil Construction
  • Industrial and General Fabrication

Welding Process

  • FCAW (Flux Core)

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded22 %620 MPa (90 ksi)435 MPa (63 ksi)

Deposition Data

Current Deposition Rate Diameter Deposition Efficiency (%) TTW Dist. Voltage Wire Feed Speed
120 A 0.8 kg/h (1.7 lb/h) 0.9 mm (.035 in.) 77 % 9.5 mm (3/8 in.) 17 V 394 cm/min (155 in./min)
200 A 2.0 kg/h (4.5 lb/h) 0.9 mm (.035 in.) 81 % 9.5 mm (3/8 in.) 17 V 995 cm/min (392 in./min)
80 A 0.4 kg/h (0.9 lb/h) 0.9 mm (.035 in.) 75 % 9.5 mm (3/8 in.) 15 V 206 cm/min (81 in./min)
150 A 1.0 kg/h (2.1 lb/h) 1.2 mm (.045 in.) 79 % 12.5 mm (1/2 in.) 17 V 300 cm/min (118 in./min)
225 A 1.2 kg/h (2.6 lb/h) 1.2 mm (.045 in.) 82 % 12.5 mm (1/2 in.) 18 V 356 cm/min (140 in./min)
95 A 0.4 kg/h (0.9 lb/h) 1.2 mm (.045 in.) 74 % 12.5 mm (1/2 in.) 15 V 137 cm/min (54 in./min)
160 A 1.0 kg/h (2.1 lb/h) 1.6 mm (1/16 in.) 78 % 16 mm (5/8 in.) 17 V 142 cm/min (56 in./min)
200 A 1.3 kg/h (2.9 lb/h) 1.6 mm (1/16 in.) 80 % 16 mm (5/8 in.) 18 V 193 cm/min (76 in./min)
275 A 2.4 kg/h (5.2 lb/h) 1.6 mm (1/16 in.) 81 % 16 mm (5/8 in.) 19 V 335 cm/min (132 in./min)
185 A 1.1 kg/h (2.4 lb/h) 2.0 mm (5/64 in.) 77 % 25 mm (1 in.) 19 V 127 cm/min (50 in./min)
250 A 2.0 kg/h (4.5 lb/h) 2.0 mm (5/64 in.) 79 % 25 mm (1 in.) 20 V 231 cm/min (91 in./min)
300 A 3.0 kg/h (6.6 lb/h) 2.0 mm (5/64 in.) 81 % 25 mm (1 in.) 21 V 343 cm/min (135 in./min)

Classifications

Classifications AWS A5.36 : E71T11-Z-CS3
AWS A5.20 : E71T-11

Approvals

Grade CSA W48 E491T-11-H16
Society CWB
Approvals are based on factory location. Please contact ESAB for more information.

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
Al C Mn P S Si
1.10 % 0.22 % 0.60 % 0.01 % 0.003 % 0.21 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Coreshield 11
242203511
242201408
242201424 Find a distributor
242201416 Find a distributor
242201507 Find a distributor

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..