STOODCOR 136 is an erosion and corrosion resistant alloy with complex carbide design well suited for hardfacing and cladding applications where erosion and corrosion are of equal concern. The ability of STOODCOR 136 to resist high abrasion in a corrosive environment makes the alloy optimal for hardfacing and cladding pipe, plate and vessels.

BUY NOW


Features

  • Optimal performance alloy for application where erosion and corrosion are of equal concern.
  • Complex carbide deposit producing chromium and fine primary carbides in an austenitic matrix.


Typical Tensile Properties

Deposition Data

Current Deposition Type Diameter TTW Dist. Voltage Wire Feed Speed
225-275 A Full Range 1.6 mm (1/16 in.) 16-19 mm (5/8-3/4 in.) 24-27 V 508-635 cm/min (200-250 in./min)
425-475 A Full Range 2.8 mm (7/64 in.) 25-32 mm (1-1 1/4 in.) 27-29 V 457-559 cm/min (180-220 in./min)

Typical Weld Metal Analysis %

C Cr Fe Other
4.0 % 24.0 % BAL % 7.5 %