SA Super 20 deposit is a very highly alloyed chromium-tungsten-moly-iron used for service involving very severe abrasive conditions and hot wear up to 1100F.

BUY NOW


Features

  • The abrasion resistance of this alloy approaches that of a tungsten carbide and thus has been given the name "the poor mans tungsten carbide".

Typical Tensile Properties

Deposition Data

Current Deposition Type Diameter TTW Dist. Voltage
200-250 A Full Range 1.6 mm (1/16 in.) 25-32 mm (1-1 1/4 in.) 24-28 V
350-500 A Full Range 2.8 mm (7/64 in.) 19-38 mm (1-1 1/2 in.) 26-30 V

Typical Weld Metal Analysis %

C Cr Fe Other
5.0 % 21.0 % BAL % 12.0 %