Nicromang deposit is a typical 13 - 16% manganese steel alloy with additions of chromium and nickel to improve its weldability and physical properties. It is primarily used for build up, repair, and joining of manganese steels.

BUY NOW


Features

  • Deposit thickness is unlimited. Nicromang can be flame cut without difficulty and it work hardens significantly under impact. Nicromang and SA Nicromang are interchangeable names for the same product.
  • Nicromang-G is a gas shielded version of 1/16" diameter Nicromang wire.


Typical Tensile Properties

ElongationTensile Strength Yield Strength
21 %820 MPa (119 ksi)615 MPa (89 ksi)

Deposition Data

Current 275-375 A
Deposition Type 3
Diameter 7/64 in.
Diameter 2.8 mm
TTW Dist. 3/4-1 1/4 in.
TTW Dist. 19-32 mm
Voltage 25-28 V

Typical Weld Metal Analysis %

C Cr Fe Mn Other
1.0 % 4.0 % BAL % 15.0 % 0.5 %