Stoody PR2009-O

Stoody

Stoody PR2009-O

The following items have been added to your list


x

Stoody PR2009 is a chromium carbide wire designed specifically for the repair of worn ID claddings in pipe elbows. PR2009 is optimized to result in superior weldability for overlaying pipe ID in the horizontal position. Special deoxidizers within PR2009 make it possible to achieve sound ID claddings when repairing worn chromium carbide overlays with hydrocarbon contamination embedded in existing relief cracks.

BUY NOW


Features

  • Designed specifically for repair of pipe and elbow ID cladding
  • Special deoxidizers make it possible to achieve sound ID claddings when repairing worn chromium carbide overlays with hydrocarbon contamination embedded within existing relief cracks


Typical Tensile Properties

Deposition Data

Current 450-500 A
Deposition Type 3
Diameter 7/64 in.
Diameter 2.8 mm
TTW Dist. 1-1 1/4 in.
TTW Dist. 25-32 mm
Voltage 28-29 V
Wire Feed Speed 180-220 in./min
Wire Feed Speed 457-559 cm/min

Typical Weld Metal Analysis %

C Cr Fe Si
5.5 % 27.0 % BAL % 2.0 %