Foundry Co-Mang is an austenitic manganese steel deposit which is suitable for multi-layer build-up and has excellent work hardening characteristics. It can also be used to join austenitic manganese steels.

BUY NOW


Typical Tensile Properties

Deposition Data

Current 200-250 A
Deposition Type 3
Diameter 1/16 in.
Diameter 1.6 mm
TTW Dist. 3/4-1 1/4 in.
TTW Dist. 19-32 mm
Voltage 24-26 V

Typical Weld Metal Analysis %

C Fe Mn Other
1.0 % BAL % 16.0 % 1.0 %