Dynamang deposit is an austenitic manganese steel containing chromium and some nickel. It produces a tough, high-strength deposit that work hardens under impact. It is primarily used for the build up, repair, and joining of manganese steel components in the cement, rock-crushing and mining industries.
BUY NOW
Features
- Alloy produces tough, high strength deposits that work harden under impact
- Primarily used for build-up, repair, and joining of manganese steel
- Deposit thickness is unlimited and can be flame cut without difficulty