Stoody

Stoody 600-O

Stoody 600-O

Particularly suited for high stress applications like cement clinker crusher rolls, Stoody 600 produces a titanium carbide bearing deposit exhibiting excellent abrasion resistance as well as toughness for good impact resistance.

Where To Buy


Features

  • Titanium carbide deposit delivering excellent abrasion resistance, with toughness and good impact resistance
  • When compared to other titanium carbide alloys, Stoody 600 exhibits good operational characteristics and excellent slag removal
  • Particularly well suited to high stress applications such as cement clinker crusher rolls


Specifications


Typical Tensile Properties

Hardness (HRC)
37-59 HRC

Typical Weld Metal Analysis %

OtherCTiCrFe
4.0 %2.0 %5.5 %8.0 %BAL %

x

Typical Tensile Properties

Hardness (HRC)
37-59 HRC

Typical Weld Metal Analysis %

OtherCTiCrFe
4.0 %2.0 %5.5 %8.0 %BAL %