Stoody 145-O
Stoody 145 offers high abrasion resistance, high corrosion resistance and high hardness at elevated temperatures thanks to Niobium content - contributes to excellent high temperature abrasion resistance up to 1500°F (816°C).
Features
- High abrasion and corrosion resistance
- Maintains hardness at elevated temperatures - up to 1500°F (816°C)
- Can be applied to carbon, low alloy, and manganese steels
Typical Tensile Properties
Deposition Data
Current | Deposition Type | Diameter | TTW Dist. | Voltage |
250-500 A | Full Range | 2.4 mm (3/32 in.) | 19-38 mm (3/4-1 1/2 in.) | 26-30 V |
300-550 A | Full Range | 2.8 mm (7/64 in.) | 19-38 mm (3/4-1 1/2 in.) | 28-30 V |
400-600 A | Full Range | 3.2 mm (1/8 in.) | 38-44 mm (1 1/2-1 3/4 in.) | 32-34 V |
Typical Weld Metal Analysis %
C | Cr | Fe | Mo | Other |
6.0 % | 24.0 % | BAL % | 6.0 % | 10.0 % |