Stoody 143-O
Stoody 143 deposits consist of primary chromium carbides and secondary Niobium carbides in an austenitic matrix exhibiting high abrasion resistance and hardness up to 1100°F
Features
- High abrasion resistance
- Maintains hardness up to 1100°F
- Can be applied to carbon, low alloy, and manganese steels
Typical Tensile Properties
Deposition Data
Current | Deposition Type | Diameter | TTW Dist. | Voltage |
170-220 A | Full Range | 1.6 mm (1/16 in.) | 10-13 mm (3/8-1/2 in.) | 24-26 V |
280-550 A | Full Range | 2.8 mm (7/64 in.) | 25-38 mm (1-1 1/2 in.) | 28-32 V |
Typical Weld Metal Analysis %
C | Cr | Fe | Other |
5.0 % | 22.5 % | BAL % | 9.0 % |