Stoody 134-O

Stoody

Stoody 134-O

The following items have been added to your list


x

Stoody 134 deposit is a high chromium-iron alloy recommended for applications subject to severe abrasion, moderate impact, and high compressive loads. It can be deposited on carbon, low alloy, and manganese steel.

BUY NOW


Features

  • Deposits are normally limited to two layers, develop cross checks, and are not machinable or forgeable. It can be used in hot wear applications up to 900F.

Typical Tensile Properties

Deposition Data

Current 300-350 A
Deposition Type 3
Diameter 7/64 in.
Diameter 2.8 mm
TTW Dist. 3/4-1 1/4 in.
TTW Dist. 19-32 mm
Voltage 26-28 V

Typical Weld Metal Analysis %

C Cr Fe Other
4.0 % 26.0 % BAL % 4.0 %