Stoody 133 deposits offer good resistance to corrosion, heat and galling and can be applied in multiple layers crack free. Deposits are machinable with carbide tools and will polish to a mirror finish in service. It can be applied to carbon, low alloy, and manganese steels.

BUY NOW


Features

  • It is recommended for parts where a low coefficient of friction is desirable and where cross checking is undesirable.
  • The 1/16" & 3/32" diameter Stoody 133 can be applied in a twin arc spray operation, producing a thermal spray coating with an excelllent balance of abrasion and corrosion resistance.


Typical Tensile Properties

Deposition Data

Current 200-300 A
Deposition Type 3
Diameter 1/16 in.
Diameter 1.6 mm
TTW Dist. 1/2-1 in.
TTW Dist. 13-25 mm
Voltage 22-26 V

Typical Weld Metal Analysis %

C Cr Fe Other
2.0 % 26.0 % BAL % 7.0 %