Stoody 131 is recommended for parts where a low coefficient of friction and minimum cross checking are desirable. Deposits provide excellent bearing surfaces on friction type guides and cement mill gudgeons. It can be applied to carbon, low alloy, and manganese steels.

BUY NOW


Features

  • Deposits are not machinable or forgeable. It is generally limited to 2 passes, although multiple layers can be applied with proper procedure (fast travel and preheat control).

Typical Tensile Properties

Deposition Data

Current Deposition Type Diameter TTW Dist. Voltage
175-225 A Full Range 1.6 mm (1/16 in.) 13-25 mm (1/2-1 in.) 24-26 V
250-350 A Full Range 2.8 mm (7/64 in.) 19-32 mm (3/4-1 1/4 in.) 24-28 V

Typical Weld Metal Analysis %

C Fe Other W
2.0 % BAL % 1.0 % 40.0 %