Stoody

Stoody 121-O

Stoody 121-O

Stoody 121 offers uniformly dispersed chromium carbides in a semi-austenitic matrix. Recommended for applications where abrasion is severe and impact is only moderate, Stoody 121 typically cross checks when applied and can be deposited on carbon, low alloy and manganese steels. Superior performance on a wide variety of heavy equipment and earth engaging tools.

Where To Buy


Features

  • Semi-austenitic matrix with uniformly dispersed chromium carbides
  • Recommended for applications with severe abrasion and only moderate impact
  • Typically cross checks upon application and not machinable
  • Can be applied to carbon, low alloy and manganese steels


Specifications


Typical Tensile Properties

Hardness (HRC)
40-51 HRC

Typical Weld Metal Analysis %

ELEMENTVALUES
OtherCCrFe
4.0 %3.0 %15.0 %BAL %

x
Stoody 121-O

Typical Tensile Properties

Hardness (HRC)
40-51 HRC

Typical Weld Metal Analysis %

ELEMENTVALUES
OtherCCrFe
4.0 %3.0 %15.0 %BAL %