Stoody 120 deposit is a high manganese alloy for applications involving wear and severe impact.

BUY NOW


Features

  • Deposits are austenitic whether applied to carbon steel or manganese steel.
  • Stoody® 120 deposits work harden, are non-magnetic, are are machinable with carbide tools, and can be flame cut.


Typical Tensile Properties

Deposition Data

Current 150-250 A
Deposition Type 3
Diameter 1/16 in.
Diameter 1.6 mm
TTW Dist. 1/2-1 in.
TTW Dist. 13-25 mm
Voltage 23-27 V

Typical Weld Metal Analysis %

C Cr Fe Mn Other
1.0 % 3.0 % BAL % 20.0 % 0.5 %