Stoody 117 deposit consists of uniformly dispersed chromium carbides in a semi-austenitic matrix that provides a deposit with good impact, abrasion, and anti-galling properties. It develops a light crosschecking patter which allows this material to be applied in multiple layers without difficulty.

BUY NOW


Features

  • It is frequently used as both a build-up and hardfacing alloy on carbon, low alloy, and manganese steels.
  • Weldability is very good and deposits are not machinable.


Typical Tensile Properties

Deposition Data

Current 300-600 A
Deposition Type 3
Diameter 7/64 in.
Diameter 2.8 mm
TTW Dist. 1 1/4-1 1/2 in.
TTW Dist. 32-38 mm
Voltage 31-35 V

Typical Weld Metal Analysis %

C Cr Fe Other
2.0 % 10.0 % BAL % 4.5 %