This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next
Stoody

Stoody 111-O

Stoody 111-O

Stoody 111-O is an open arc wire that produces a austenitic chromium manganese steel deposit containing alloy carbides. Stoody 111-O deposit is used in the rebuilding of manganese steel parts subject to severe impact loading combined with abrasion. The abrasion resistance of Stoody 111-O deposit is 5-6 times superior to that of an austenitic manganese deposit as measured in the G65 test. This material offers good toughness and wear resistance, and is sometimes used as the final hardfacing layer in extreme impact situations. It can be used on carbon and manganese steels.

Where To Buy


Specifications


Typical Tensile Properties

Hardness (HRC)
30-49 HRC

Typical Weld Metal Analysis %

OtherMnCCrFe
1.0 %15.5 %2.0 %12.5 %BAL %

x

Typical Tensile Properties

Hardness (HRC)
30-49 HRC

Typical Weld Metal Analysis %

OtherMnCCrFe
1.0 %15.5 %2.0 %12.5 %BAL %