Stoody 111-O is an open arc wire that produces a austenitic chromium manganese steel deposit containing alloy carbides. Stoody 111-O deposit is used in the rebuilding of manganese steel parts subject to severe impact loading combined with abrasion. The abrasion resistance of Stoody 111-O deposit is 5-6 times superior to that of an austenitic manganese deposit as measured in the G65 test. This material offers good toughness and wear resistance, and is sometimes used as the final hardfacing layer in extreme impact situations. It can be used on carbon and manganese steels.

BUY NOW


Typical Tensile Properties

Deposition Data

Current 300-400 A
Deposition Type 3
Diameter 7/64 in.
Diameter 2.8 mm
TTW Dist. 1-1 1/2 in.
TTW Dist. 25-38 mm
Voltage 26-27 V

Typical Weld Metal Analysis %

C Cr Fe Mn Other
2.0 % 12.5 % BAL % 15.5 % 1.0 %
x

Part Numbers and Accessories

Select All | Select None

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..