Stoody 105-O
Stoody 105-O deposit is a low alloy steel developed for rebuilding carbon and low alloy steel parts used on applications involving metal to metal wear. Multiple layer crack free deposits can be obtained. When more than three layers are required, an under base of Stoody 104 is recommended. Stoody 105-O requires carbide tools for machining along with rigid well-powered equipment. It is good for hot wear applications up to 600° F.
Deposition Data
Current | 200-350 A |
Deposition Type | 3 |
Diameter | 3/32 in. |
Diameter | 2.4 mm |
TTW Dist. | 3/4-1 1/4 in. |
TTW Dist. | 19-32 mm |
Voltage | 24-28 V |
Typical Weld Metal Analysis %
C | Cr | Fe | Other |
0.5 % | 3.0 % | BAL % | 4.0 % |