Stoody 102-O
Stoody 102 deposit has a composition and physical properties that are similar to those of H-12 tool steel. Weldability is very good and the wire can be applied out-of-position. Stoody 102 requires carbide tools for machining. It is good for hot wear applications up to 1100F.
Features
- Multiple layers can be applied without difficulty when proper preheat and interpass temperatures are maintained.
Typical Tensile Properties
Deposition Data
Current | 225-275 A |
Deposition Type | 3 |
Diameter | 1/16 in. |
Diameter | 1.6 mm |
TTW Dist. | 1/2-1 in. |
TTW Dist. | 13-25 mm |
Voltage | 25-27 V |
Typical Weld Metal Analysis %
C | Cr | Fe | Other |
0.5 % | 8.0 % | BAL % | 6.0 % |