Low alloy TIG rod for repairing medium and high carbon steels where complete heat treatment is desired such as SAE 4130, 4140, 4330, 4340, 8620, and 8630 steels. Hardness from 36 to 38 Rockwell C. Copper coated.

BUY NOW


Specifications


Typical Tensile Properties

Condition Hardness (HRC) Tensile Strength
As Welded 36-38 HRC 138-163 ksi