Specifications


Typical Tensile Properties

Condition Elongation Hardness (BHN) Tensile Strength Yield Strength
As Welded 22-25 % 22-22 BHN up to 120 ksi up to 90 ksi

x

Typical Tensile Properties

Condition Elongation Hardness (BHN) Tensile Strength Yield Strength
As Welded 22-25 % 22-22 BHN up to 120 ksi up to 90 ksi

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State 275
A/S 275 3/16X14X10X40#VALP 69010073 Buy Local
A/S 275 1/8X14X5#X40# 69015071 Buy Local
A/S 275 3/32X9X5X20#VALP 69010070 Buy Local
A/S 275 1/8X14X10X40#VALP 69010071 Buy Local
A/S 275 5/32X14X10X40#VALP 69010072 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..