An AC/DC reverse, all-position electrode producing an outstanding bead appearance. Use on tool,high alloy, aircraft, spring, nickel-clad, stainless, and dissimilar steels. Excellent for dirty, greasy, and rusty metals. Machinable.

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 22-25 % up to 120 ksi 94 ksi

x

Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 22-25 % up to 120 ksi 94 ksi

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State 275 SUPER
A/S SUPER 275 1/8X14X5X40#VALP 69200030 Buy Local
A/S SUPER 275 1/8X14X10X40 69200012 Buy Local
A/S 275 SUPER 3/32X9X1#X10 69201011 Buy Local
A/S SUPER 275 DSPL PK (7RODS) 69001002 Buy Local
A/S SUPER 275 3/32X9X5X20#VALP 69200011 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..