Previous Next
ESAB

All-State 252

All-State 252

This AC/DC reverse, all-position electrode is used for welding 310 and 314 stainless subjected to corrosion and elevated temperatures, as well as dissimilar steels and stainless of unknown analysis.

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Hardness (HRC) Tensile Strength Yield Strength
As Welded 35-45 % B85-B85 HRC 95 ksi 65 ksi

x

Typical Tensile Properties

Condition Elongation Hardness (HRC) Tensile Strength Yield Strength
As Welded 35-45 % B85-B85 HRC 95 ksi 65 ksi

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State 252
A/S 252 1/8X14X10X40 69010062 Buy Local
A/S 252 1/8X14X5#X40#VALP 69015062 Buy Local
A/S 252 3/32X9X5X40#VALP 69010061 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..