All-State Shield-Free Plus-SP

Self-shielding flux cored wire. No gas required. All-position, DC straight polarity. Ideal for thin gauged galvanized and mild steels, light to moderate rusty steels. Welds over oil ,grease, and mill scale. Single pass only. Meets AWS A5.20 Class E71T-GS

BUY NOW


Specifications


Typical Tensile Properties

Condition Tensile Strength
As Welded 76 ksi

x

Typical Tensile Properties

Condition Tensile Strength
As Welded 76 ksi