All-State Bi-Metal

Silver brazing alloy with a layer of All-State 164 Silver Brazing alloy laminated to each side of the composition metal forming a .02 (.5mm) thick strip. For tungsten carbides, stainless, and high alloyed steels. Absorbs shock and stress. Use with All-State No. 110 flux or All-State S-200 flux

Where To Buy


Specifications


Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 55 ksi 1500 °F

x

Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 55 ksi 1500 °F

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State Bi-Metal
A/S BI-METAL 020X1 X1 EACH 69050220 Buy Local