All-State 155All-State 155'

ESAB

All-State 155

All-State 155

A cadmium free food grade brazing alloy with low melting temperature. For joining and repair of steels, stainless steels, nickel, copper, and high speed steels. Use with All-State No. 110 flux or All-State S-200 flux 56% Silver

BUY NOW


Specifications


Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 50 ksi 1150-1200 °F

x

Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 50 ksi 1150-1200 °F

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State 155
A/S 155 1/16X2OZ COILX12 69050190 FIND A DISTRIBUTOR
A/S 155 1/16X4OZ COILX12 69050191 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..