45% silver brazing alloy for use on light gauge material and tight fitting joints. Excellent capillary flow on ferrous and non-ferrous metals or combinations of both (excluding white metals). Excellent for food processing or food handling equipment. Use with All-State No. 110 or All-State S-200 flux.

Where To Buy


Specifications


Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 75 ksi 1225-1370 °F

x

Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 75 ksi 1225-1370 °F

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State 101 CDFR
A/S 101 CD FR 1/16 X 2 OZ COIL 69050352 Buy Local
A/S 101 CD FR 1/16X1# COIL 69050354 Buy Local
A/S 101 CD FR KIT 1/16 110 4OZ 69050179 Buy Local
A/S 101 CD FR KIT 1/16 110 2OZ 69050178 Buy Local
A/S 101 CD FR 1/16X4OZ COILX3# 69050353 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..