All-State 100

ESAB
All-State 100

A cadmium free nickel bearing food grade silver brazing alloy for stainless steel, carbide tools, and for joining ferrous and nonferrous metals (except white metals) 40% Silver.

BUY NOW


Specifications


Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 60 ksi 1250-1400 °F