Stoody 87TG
Stoodys torch grade spray powders are specifically designed for enhanced wetting characteristics in hand-held torch applications. These hardfacing powers cover a broad range of wear resistance needs.
Features
- A nickel-base alloy with outstanding resistance to abrasion, corrosion and high heat: impact resistance is good.
- Low coefficient of friction, Used for pump components, shaft sleeves, thrust collars, guides, bushings.
- Finish by grinding.

Documents
Typical Weld Metal Analysis %
C | Cr | Fe | Ni | Other |
0.5 % | 5.0 % | 2.0 % | BAL % | 3.0 % |