Stoody

Stoody 64TG

Stoody 64TG

Stoodys torch grade spray powders are specifically designed for enhanced wetting characteristics in hand-held torch applications. These hardfacing powers cover a broad range of wear resistance needs.

Where To Buy


Features

  • A nickel-base alloy with outstanding resistance to abrasion, corrosion and high heat: impact resistance is good.
  • Low coefficient of friction, Used for pump components, shaft sleeves, thrust collars, guides, bushings.
  • Finish by grinding.


Specifications


Typical Weld Metal Analysis %

OtherCNiCrFe
5.0 %0.5 %BAL %9.0 %4.0 %

x
Stoody 64TG

Typical Weld Metal Analysis %

OtherCNiCrFe
5.0 %0.5 %BAL %9.0 %4.0 %

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Stoody 64TG
64TG Spray Powder 5lb Bottle 11020700 Buy Local