All-State RG-45

(Copper Finish) For oxy-fuel welding on steel plate,sheet and pipe wrought iron where strength up to 45 ksi is required. Meets AWS A5.2, Class R45

Where To Buy


Specifications


Typical Tensile Properties

Condition Tensile Strength
As Welded 45 ksi

x

Typical Tensile Properties

Condition Tensile Strength
As Welded 45 ksi

x