All-State 11FC'

ESAB

All-State 11FC

All-State 11FC

A high strength brazing alloy for joining ferrous and non-ferrous metals (except white metals), and carbon and alloy steels. Higher strength than ordinary bronze rods, can replace many higher cost silver alloys.

BUY NOW


Specifications


Typical Tensile Properties

500 kg. load
Condition Hardness (BHN) Tensile Strength Working Temperature
As Welded 90-110 BHN up to 85 ksi 1200-1750 °F

x

Typical Tensile Properties

500 kg. load
Condition Hardness (BHN) Tensile Strength Working Temperature
As Welded 90-110 BHN up to 85 ksi 1200-1750 °F

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State 11FC
A/S 11FC 1/8X18X3X48 69050021 FIND A DISTRIBUTOR
A/S 11FC 1/8X18X10X40 69051020 FIND A DISTRIBUTOR
A/S 11FC 3/32X18X3X48 69053020 FIND A DISTRIBUTOR
A/S 11FC 3/32X18X10X40 69050020 FIND A DISTRIBUTOR
A/S NO.11FC3/32 DSPLPK(10RODS) 69001007 FIND A DISTRIBUTOR