All-State Paste Solder

A 50/50 lead/tin solder for sealing, joining or tinning most common metals, except aluminum. Can be used with soldering iron or torch. Working temperature is 360°F to 375°F.

Where To Buy


Specifications


Typical Tensile Properties

Condition Tensile Strength
As Welded up to 6 ksi