An intermediate temperature range solder for zinc base die castings. Will produce smooth, dense, porosity free deposits that will color match on zinc die castings.

Where To Buy


Specifications


Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 28 ksi 371 °C