VANCAR weld deposits contain vanadium carbides, with a wear resistance similar to that of tungsten carbide but with superior impact resistance. A unique feature of this alloy is that the vanadium carbides dissolve and reform in the weld deposit creating an even distribution.

BUY NOW


Features

  • Vanadium carbides dissolve and reform in the weld deposit resulting in even distribution
  • Exhibits wear resistance close to that of tungsten carbine but with superior impact resistance


Deposition Data

Current Deposition Type Diameter TTW Dist. Voltage
200-300 A Full Range 2.4 mm (3/32 in.) 25-32 mm (1-1 1/4 in.) 25-27 V
150-200 A Full Range 1.6 mm (1/16 in.) 13-19 mm (1/2-3/4 in.) 22-26 V

Typical Weld Metal Analysis %

C Fe Other V W
3.9 % BAL % 3.0 % 16.0 % 6.0 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Stoody VANCAR-O
11420200 FIND A DISTRIBUTOR
11333700 FIND A DISTRIBUTOR
11904300 FIND A DISTRIBUTOR
11420100 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..