Stoody Vancar-E
Stoody Vancar E is a coated fabricated electrode that contains specially formulated vanadium tungsten carbide particles approximately equal to tungsten carbide in hardness but at only half the density. Vancar has an advantage over tungsten carbide because it can be applied in multiple layers and still retain its original hardness due to uniform distribution of the carbide particles.
Features
- This provides wear rates that remain uniform throughout the life of the deposit.
Deposition Data
Current | Deposition Type | Diameter |
130-165 A | Full Range | 4.8 mm (3/16 in.) |
80-130 A | Full Range | 4.0 mm (5/32 in.) |
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||
C | Fe | Mn | Mo | Ni | Si | V | W | |||||||
4.9 % | Bal % | 0.8 % | 0.8 % | 0.5 % | 2.1 % | 18.0 % | 10.0 % |