Stoody

Stoody Horseshow Borium

Stoody Horseshow Borium

Stoody Horseshoe Borium was developed to provide a maximum non-slipping surface when applied to horseshoes. It is manufactured by metering relatively large tungsten carbide particles into steel.

Where To Buy


Specifications


Typical Weld Metal Analysis %

OtherCWFe
0.1 %2.5 %57.0 %BAL %

x

Typical Weld Metal Analysis %

OtherCWFe
0.1 %2.5 %57.0 %BAL %