Stoody ATB
Bare Acetylene Tube Borium is an oxy-fuel rod intended for metal-to-earth applications involving extreme abrasion and low impact. It is manufactured by metering crushed tungsten carbide particles of controlled mesh size into steel tubes.
Features
- Borium is available in a variety of particle sizes - fine mesh sizes increase wear resistance and coarse sizes improve cutting efficiency.
Deposition Data
Deposition Type | Diameter |
Full Range | 4.0 mm (5/32 in.) |
Full Range | 4.8 mm (3/16 in.) |
Full Range | 3.2 mm (1/8 in.) |
Typical Weld Metal Analysis %
C | Fe | Other | W |
2.5 % | BAL % | 2.0 % | 57.0 % |