Stoody AC-DC Tube Borium

Stoody AC-DC Tube Borium

Stoody AC-DC Tube Borium coated electrode is manufactured by metering crushed tungsten carbide particles of controlled mesh size into steel tubes. It receives a thin graphitic coating.

Where To Buy


Features

  • The tungsten carbide particles are available in a variety of sizes - fine mesh size increases wear resistance and coarse improves cutting efficiency.
  • The tungsten carbide content (by weight) is approximately 60%.


Specifications


Typical Weld Metal Analysis %

OtherCWFe
1.5 %2.5 %BAL %39.0 %

x

Typical Weld Metal Analysis %

OtherCWFe
1.5 %2.5 %BAL %39.0 %

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Stoody AC-DC Tube Borium
1/8 in / 3.2 mm x 14 AC-DC TB CTD 10lb Vacpak 10229100 Buy Local
3/16 in / 4.8 mm x 14 AC-DC TB CTD 10lb Vacpak 10229500 Buy Local
1/4 in / 6.4 mm x 14 AC-DC TB CTD 10lb Pak 10229700 Buy Local
5/32 in / 4.0 mm x 14 AC-DC TB CTD 10lb Vacpak 10229300 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..