Stoody AC-DC BOROD

Stoody AC-DC BOROD

Stoody AC-DC Borod coated electrode is used for metal-to-earth applications requiring extreme abrasion resistance and low impact resistance. It is similar to Stoody AC-DC Tube Borium in all respects except that the mesh size is finer (40 - down) to provide deposits resembling fine grit sandpaper. The finer mesh size generally provides slightly increased wear protection.

Where To Buy


Specifications


Typical Weld Metal Analysis %

OtherCWFe
2.0 %2.5 %58.0 %BAL %

x

Typical Weld Metal Analysis %

OtherCWFe
2.0 %2.5 %58.0 %BAL %