Stoody 160FC wire deposit consists of tungsten carbide particles in a nickel silicon boron matrix. Due to higher tungsten carbide content, Stoody 160FC is an ideal hardfacing overlay with a microstructure that delivers superior toughness and resistance to corrosion and fine particle erosion in slurry type applications. Stoody 160FC also provides improved weldability through enhanced wetting, tie-in, and arc stability.

Where To Buy


Features

  • Stoody 160FC microstructure delivers significant abrasion resistance as well as superior toughness and corrosion resistance.
  • Well suited for upstream oil and gas production applications and as an overlay for the more ductile build up alloys like Stoody 155FC.
  • Designed for the GMAW welding process, Stoody 160FC can be applied at a much lower voltage and heat input resulting in reduced interpass temperatures and levels of distortion in the component.


Specifications


Typical Tensile Properties

75% Ar - 25% CO2
Hardness (HRC)
38-45 HRC

Typical Weld Metal Analysis %

OtherCWNiFe
2.0 %2.0 %48.0 %BAL %0.5 %

x

Typical Tensile Properties

75% Ar - 25% CO2
Hardness (HRC)
38-45 HRC

Typical Weld Metal Analysis %

OtherCWNiFe
2.0 %2.0 %48.0 %BAL %0.5 %

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Stoody 160FC
1/16 in / 1.6 mm Stoody 160FC 33# Wire Basket 12022500 Buy Local
3/32 in / 2.4 mm Stoody 160FC 50lb PP 12027100 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..