Stoody

Stoody 160FC/160FC-O

The following items have been added to your list


x

Stoody 160FC wire deposit consists of tungsten carbide particles in a nickel silicon boron matrix. Due to higher tungsten carbide content, Stoody 160FC is an ideal hardfacing overlay with a microstructure that delivers superior toughness and resistance to corrosion and fine particle erosion in slurry type applications. Stoody 160FC also provides improved weldability through enhanced wetting, tie-in, and arc stability.

BUY NOW


Features

  • Stoody 160FC microstructure delivers significant abrasion resistance as well as superior toughness and corrosion resistance.
  • Well suited for upstream oil and gas production applications and as an overlay for the more ductile build up alloys like Stoody 155FC.
  • Designed for the GMAW welding process, Stoody 160FC can be applied at a much lower voltage and heat input resulting in reduced interpass temperatures and levels of distortion in the component.


Typical Tensile Properties

Shielding Gas
75% Ar - 25% CO2

Deposition Data

Current Deposition Type Diameter TTW Dist. Voltage Wire Feed Speed
75% Ar - 25% CO2
130-200 A Full Range 1.6 mm (1/16 in.) 13-16 mm (1/2-5/8 in.) 17-18 V 279-432 cm/min (110-170 in./min)
250-325 A Full Range 2.4 mm (3/32 in.) 16-25 mm (5/8-1 in.) 18-21 V 203-356 cm/min (80-140 in./min)

Typical Weld Metal Analysis %

C Fe Ni Other W
2.0 % 0.5 % BAL % 2.0 % 48.0 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Stoody 160FC/160FC-O
12022500 FIND A DISTRIBUTOR
12027100 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..