Stoody 160-E coated electrode consists of tungsten carbide particles in a nickel silicon boron matrix. This microstructure gives Stoody 160-E sufficient toughness, extreme abrasion resistance, and excellent fine particle erosion resistance in slurry type applications.

BUY NOW


Features

  • Sufficient toughness
  • Extreme abrasion resistance
  • Excellent fine particle erosion resistance in slurry type applications


Typical Tensile Properties

Deposition Data

Current 130-155 A
Deposition Type 3
Diameter 3/16 in.
Diameter 4.8 mm

Typical Weld Metal Analysis %

C Fe Ni Other W
2.9 % 0.5 % BAL % 2.0 % 53.0 %