This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next
Stoody

Stoody 140

Stoody 140

Stoody 140 wire consists of tungsten carbide particles in a nickel chrome boron matrix. This microstructure gives Stoody 140 superior toughness, corrosion and excellent fine particle erosion resistance in slurry type applications.

Where To Buy


Specifications


Typical Tensile Properties

75% Ar - 25% CO2
Hardness (HRC)
50-60 HRC

Typical Weld Metal Analysis %

OtherCWNiCr
1.0 %2.0 %38.0 %BAL %11.5 %

x

Typical Tensile Properties

75% Ar - 25% CO2
Hardness (HRC)
50-60 HRC

Typical Weld Metal Analysis %

OtherCWNiCr
1.0 %2.0 %38.0 %BAL %11.5 %

x
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x